Glass transition in CDW system o-TaS_3 (CROSBI ID 738826)
Prilog sa skupa u časopisu | izvorni znanstveni rad
Podaci o odgovornosti
Biljaković, Katica ; Starešinić, Damir ; Hosseini, Khalil ; Bruetting, Wolfgang
engleski
Glass transition in CDW system o-TaS_3
We report on the experimental evidence of a glass transition in the CDW phase of orthorhombic TaS_3 at T_g~50 K, brought by means of dielectric constant measurement. The relaxational mode exhibits in this T-range a critical slowing down instead of an expected activated behavior. New processes appear below the glass transition temperature which we attribute to the defect dynamics. There is an apparent similarity with the scenario of freezing out in supercooled liquids. However, the peculiarity of this glass transition is a very large length scale of order of mu m (beyond the phase coherence length of the underlying CDW), compared to nm in supercooled liquids.
charge-density-wave systems; glass transitions; dielectric permittivity; dielectric loss and relaxation
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
nije evidentirano
Podaci o prilogu
2616-2619-x.
1999.
nije evidentirano
objavljeno
Podaci o matičnoj publikaciji
Synthetic metals
0379-6779
Podaci o skupu
Nepoznat skup
ostalo
29.02.1904-29.02.2096