Kinetic analysis of the thermooxidative degradation of poly(vinyl-chloride)in poly(viny chloride)/methyl methacrylate-butadiene-styrene blends.2.Nonisothermal degradation (CROSBI ID 94165)

Prilog u časopisu | izvorni znanstveni rad | međunarodna recenzija

Andričić, Branka ; Kovačić, Tonka ; Klarić, Ivka Kinetic analysis of the thermooxidative degradation of poly(vinyl-chloride)in poly(viny chloride)/methyl methacrylate-butadiene-styrene blends.2.Nonisothermal degradation // Polymer degradation and stability, 79 (2003), 265-270-x

Podaci o odgovornosti

Andričić, Branka ; Kovačić, Tonka ; Klarić, Ivka

engleski

Kinetic analysis of the thermooxidative degradation of poly(vinyl-chloride)in poly(viny chloride)/methyl methacrylate-butadiene-styrene blends.2.Nonisothermal degradation

The process of thermooxidative degradation of poly (vinyl chloride)/(methyl methacrylate-butadiene-styrene) (PVC/MBS) blends was investigated by means of nonisothermal thermogravimetry in air. Measurements were carried out in the temperature range of 50-650°C. The kinetic parameters (Ea and A) of the first degradation step were determined by applying Flynn-Wall-Ozawa method. Their relationship through compensation effect was discussed and the apparent compensation effect was found. The addition of MBS changes the rate of PVC dehydroclorination in the blends, while in the blends with 15 and more MBS ratio, the reaction scheme of degradation changes too.

nonisothermal kinetics; PVC/MBS blends; thermooxidative degradation

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

nije evidentirano

Podaci o izdanju

79

2003.

265-270-x

objavljeno

0141-3910

Povezanost rada

Kemijsko inženjerstvo

Indeksiranost